Re: [MW:12292] PDR for welder overlay on flanges

1)Yes.
2)Yes.

I assume that these flanges are part of nozzles.
Permanent blind flanges which are part of Vessels shall also be U-part stamped if overlayed by welding.( Example: Manway blinds)

Arunachalam

On Fri, Aug 19, 2011 at 8:44 PM, imran khan <imransian@gmail.com> wrote:
Dear All,
 
we are pressure vessel manfacturer  having U - Stamp , we purchase some flanges of carbon steel  which are overlayed, But the supplier did not provide PDR
my question is ,
 
1) Is it required?(Section VIII div. 1 addition 2007)
2)Does the flanges should be stamped "U"

--
With Best Wishes,
 
Imran
 
   

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arunachalam.A,
Abu Dhabi Gas Industries Ltd,
P.O.Box # 50124
Abu Dhabi, UAE
Mobile : +971-50-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...