Re: [MW:11995] AISI 4145

Ashish,

We have in our facility the welding processes like SMAW, SAW, GTAW & GMAW. The reason behind to quality PQR is to weld AISI 4145 Base material for build up and machine back to drawing required dimensions.
Ashish you are right, this material can be used for Tool joints, Drill pipe and Collars manufacturing purposes,because it meets to API minimum Yield strength requirements.


Regards,
Mubeen
+966-565013851



On Fri, Jul 29, 2011 at 9:05 PM, ashish baviskar <ashishqci@gmail.com> wrote:
dear Mubeen,
                        Please tell me which type of welding you are going to use . Whether it is SAW or SMAW or FCAW ? AISI 4145 material are mostly use in API spec 7 , 7-1 products like drill collars, drill pipes , subs etc. and also tell me the application. 


On Fri, Jul 29, 2011 at 10:01 AM, mubeen mubeen <mubeenaws@gmail.com> wrote:
Hi,

Can anybody help me out in order to weld subject base material with appropriate consumables(Electrode or filler wire), along with its preheat and post weld heat treatment temperatures.

Regards,
Mubeen
QA Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ASHISH BAVISKAR
SURVEYOR
ABSIV INDIA PVT LTD.
(ABS Consulting )
CONTACT NO: 9222180936

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...