Friday, July 29, 2011

Re: [MW:11970] Orbital Welding

Dear Sir, 

You can contact  MAGNATECH INTERNATIONAL BV . They have wide range of welding machines for orbital as well as pipeliners. 

With regards. 

AG

On Wed, Jul 27, 2011 at 5:41 PM, Ahmed Husain <ahmraha@yahoo.com> wrote:
Hi,
 
Contractor at our current project used orbital welding for field work, but it was not very successful. Moving machine to every job location and set was time consuming. Also welding operators had to go for extensive training to produce satisfactory welds.  

 

Ahmed Husain
 




From: Izhar Mustafa <izharmustafa@gmail.com>
To: materials-welding@googlegroups.com
Cc: srinivassirigineedi@gmail.com
Sent: Mon, July 25, 2011 7:06:51 PM
Subject: Re: [MW:11920] Orbital Welding

Hi Srinivas,

Thanks, Can u tel r u using these machines, which model? What is repair percentage in RT? what are the major factor for good Orbital machines to get low repair rate, How u r achieving proper fit-up for Orbital welding as i know main factor of orbital welding is proper and accurate fit-up.


Regards

Izhar


On Mon, Jul 25, 2011 at 1:13 PM, Srinivas <srinivassirigineedi@gmail.com> wrote:

AMI MACHINES, good performance but costly

Cheers,
Srinivas
Sent from my iPhone 4

On 24-Jul-2011, at 8:03 PM, Izhar Mustafa <izharmustafa@gmail.com> wrote:

Dear Experts,

Can anyone have experience of Orbital welding GTAW from 2" to 14". Pl share practical experience with Machine info.
Will be thankful.

Regards

Izhar 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ABHISHEK GHOSH
FAHAHEEL, KUWAIT
MOB: (00)965-65772043

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...