Hi venkateswaran
 
1) PWHT as per UCS-56 is mandatory for welded joints over 38 mm nominal thickness.

2)  for welded joints of  nominal thickness over 32 mm through 38 mm, PWHT is not required if  preheat is applied at a
minimum temperature of 95 degree celcius during welding.
 
Please go through all the notes, in UCS-56 for exceptions.
 
Thanks
 
Murugesan

On Sat, Jun 25, 2011 at 3:14 PM, Venkateswaran <k.venkateswaran@ionexchange.co.in> wrote:
Dear All
As per ASME Sec 8,what will be the minimun thickness requirement to carryout  PWHT for CS .Kl.refer me the page no/Table.
 
Regards,
K.Venkateswaran.

zero b footer 

Please consider the environment before printing this E-mail


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...