Hello everyone!
I have to inspect 132mm thickness SAW welding, CrMoV material
according API 934 for reheating cracks using TOFD.
If I didnt get wrong, I have to calibrate the system in the ASME Block
with the SDH and then adjust the gain on API block with the notches,
right??
Another doubt is about the crack characterization... its commom to
detect some porosity, even on transversal scanning, how we will judge
some signal to be reheating crack?
Thanks for the help.


Paulo

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...