Gents,
we are fabricating a Pipe line for Natural gas . Now the contractor has done Primer on Joints also before the NDT testing.

How it is going to affect it & what are the remedy for that.

--
Thanks & Regards
 
Dheerendra Singh Chauhan
Project Manager
Powergas International
+234-7055215480

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...