Friday, May 27, 2011

RE: [MW:11159] welding consumable of S 355 JR

Dear Manoj,
 
It depends what process you use for welding.
 
for SMAW:
E7018-1 (E46 5 32 H5) as example OK 55.00 from ESAB

for FCAW:
E71T-1, E81T-1 as example OK 15.13/15.18 from ESAB would be ideal for this grade of steel.
 
regards,
Elshan.

Date: Thu, 26 May 2011 17:17:34 +0400
Subject: [MW:11157] welding consumable of S 355 JR
From: manojacgnr@gmail.com
To: materials-welding@googlegroups.com

Dear All,

Which electrode i can use  to weld S355 JR to S 355 JR for SMAW process?

Thanks & Regards.

Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...