Part H AWS D1.6 says that the prequilified section is applied to the nominally austenite stainless steel listed in table 3.2.
In my case a material spec is ASTM A240 type 409 which is a ferritic stainless steel and is not on the table 3.2.
So i wanted to go with section 4 qualification. but the problem is the material thickness (thickness of test coupon) available.
what tests i can do?
> Date: Mon, 25 Apr 2011 07:11:27 -0700
> Subject: [MW:10844] Re: new WPS for 3 mm ss plate qualification
> From: fred.schweighardt@airliquide.com
> To: materials-welding@googlegroups.com
>
> I believe you should be in AWS D1.6, for structural stainless. There
> is an option for prequalificaiton in this code, which means you do not
> have to make a PQR and the associated tests
>
> On Apr 25, 5:57 am, Martin Prad <martin_p...@hotmail.com> wrote:
> > Dear friends,
> >
> > What tests are required for generating of new WPS for 3 mm ss plate?
> > Qualification code is AWS D1.1
> > Available material for welding is 3 mm ss plate.
> > Welding process is TIG.
> >
> > best regards,
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment