Thursday, March 31, 2011

Re: [MW:10535] Welder Qualification

Yes , u can use UT instead of RT
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
Sent: Wednesday, March 30, 2011 8:58 PM
Subject: [MW:10529] Welder Qualification

Dear all experts,
 
Can we qualify welder by UT?

 
Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...