Re: [MW:10012] Ineduquate cross penetration (ICP)

Dear colleague

Your piping fitting is A234 WPB. Am I correct?

All products furnished to A 234 standard shall be manufactured in accordance to the section 6 of A234. The section 6 says that all welds shall be radiography examined in accordance with article 2, ASME V with acceptance criteria in accordance with section UW-51 of ASME VIII.

For repair, see specification A960.

However, to the best of my understanding, the repair welding should only be done by the manufacturer (not by purchaser). 

Other things is; how come an ICP occur? As far I know, all product furnished under this specification have been tested and meet to the acceptance limit. I can say, all products are good quality before delivered to the purchaser. I trust you have the copy of mill test certificate.

i recommend you to raise an SQ (site query).Take a careful on this.

 

Let this helps.

Fitya a

2011/2/24 Muhammad Asif <masif_atiqui@yahoo.com>

Dear sir,
 
I have elbows which have to be used in cross country pipe line but they have contiuous (ICP) in its longitudnal seam.Can any body guid me how to resolve this issue instead of change them and also tell me the ERW elbows welding acceptence criteria.
Elbow description is under:
Dia = 28" ,Long radius,ERW, 90 degree,WPB
 
 
Asif

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...