Re: [MW:10011] welding of GI ( galvanized iron) material

Dear Maninder

You may find attached docs useful regarding welding of GI.

regards

yogesh


On 2/24/11, james gerald <gerry_tup@yahoo.com> wrote:
> Welding Galvaised steel is similar to welding any carbon steel. One option
> to reduce health Hazard, the Zinc coating can be removed from the weld joint
> and surronding area by grinding or using Emery paper. Then carry out the
> welding.
>
>
> J.GERALD JAYAKUMAR
> 00919344954677
>
>
> --- On Wed, 2/23/11, Manindra Singh <hellmanya@in.com> wrote:
>
>
> From: Manindra Singh <hellmanya@in.com>
> Subject: [MW:9981] welding of GI ( galvanized iron) material
> To: materials-welding@googlegroups.com
> Date: Wednesday, February 23, 2011, 8:16 AM
>
>
>
>
> Dear colleagues
> Please let me know about the details of welding of GI ( galvanized iron)
> material & its pros and cons.
>
> M P Singh
> Inspection Engineer
>
>
>
> Dear materials-welding! Get Yourself a cool, short @in.com Email ID now!
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...