Re: [?? Probable Spam] *****POSSIBILITE DE SPAM***** [MW:9009] E -7018 (TAPPER BURNING)

Dear Jignesh
 
THis problem is due to bad quality of coating that can't support the continous energy to the limit and this makes difference between brands .I guess the problem appears most on hig alloyed electrodes .
 
Best regards
 
Moez
----- Original Message -----
Sent: Wednesday, December 29, 2010 4:03 PM
Subject: [?? Probable Spam] *****POSSIBILITE DE SPAM***** [MW:8989] E -7018 (TAPPER BURNING)

Can anybody write some technical reasons behind tapper burning of subject electrodes with high fluctuations of current and wastage of excessive stub length because of red hot (@ 30%)?
 
Also with above, what could be the possible defects in the weld joints?
 
Regds/Jignesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...