Re: [MW:8990] E -7018 (TAPPER BURNING)

Dear Jignesh,
 
when electrode is manufacured, if the cake ( wet flux) is not concentic to core wire, this problem is possible.Hence you get problem like taper buring.Problem is weld- is porosity .
 
Better to replace.
Regards,
 
Manish Kulkarni

--- On Wed, 29/12/10, Jignesh Desai <jignesh.desai.met@gmail.com> wrote:

From: Jignesh Desai <jignesh.desai.met@gmail.com>
Subject: [MW:8989] E -7018 (TAPPER BURNING)
To: materials-welding@googlegroups.com
Date: Wednesday, 29 December, 2010, 8:33 PM

Can anybody write some technical reasons behind tapper burning of subject electrodes with high fluctuations of current and wastage of excessive stub length because of red hot (@ 30%)?
 
Also with above, what could be the possible defects in the weld joints?
 
Regds/Jignesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...