Re: [MW:8955] IQI


Greeting,

Do not confuse with all the tables you have. Refer only the table which are applicable to your job by code of constructions are as detailed out in the procedure.

Refer to your procedure or code of constriction (as some code required to add reinforcement when you selecting the IQI)

Different code have different Tables.. Generally all are follow the 2% sensitivity requirement in case of wire type IQI and 2-2T in case of plaque type IQI.

 

For selecting the wire or plate type IQI first calculate the 2% (if sensitivity requirement is 2%) of the job thickness under testing. Refer that number in the table which will give you the value for the designated required wire or plate type IQI and the wire set in which the wire include.(many time you will not find exact no so select the smallest wire diameter wire available to your calculated values)

 

Still you have some doubt send me your joint details and code/specification applicable .I can help you selecting the wire.

Better get the technique sheet write and approved by level-iii/experienced people where you will find all the relevant information.

Regards, Bhaskar kale

bmkale@gmail.com

 


On Mon, Dec 27, 2010 at 1:26 AM, Ahmed Elias <alyassahmed@gmail.com> wrote:
Thanks Gamne Krishnar,
 
        My question was not clear  there's any formula(relation between the wall thickness and wire diameter) because I have many table(see the attached file) similar to your table.
 
 Thanks for your help


 
On Sun, Dec 26, 2010 at 11:09 AM, Kisan Gamane <kisankrishna1506@gmail.com> wrote:
Dear Ahmed
Pls. find attached details which will helps to u.
 
Thanks & regards
 
Gamne Krishna
Nasik India
 


 
On Sat, Dec 25, 2010 at 6:21 PM, ahmed muhammad <alyassahmed@gmail.com> wrote:
Dear All,
   I need the way to slect the IQI for radiographic film

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

किसन गामणे

नाशिक

जन्मलो म्हणून जगणार नाही
अन असाच राखेत विरणार नाही...
ठसे सोडूनी जाईन जीवन काठावरती
आल्या लाटा कितीही , मिटणार नाही ...

 

खुभी नाही माझ्यात एवढी  कि..!
कुणाच्या  हृदयात ठाण  मांडून  जाईल..!
पण विसरणे सुद्धा अशक्य होईल..!
असे  क्षण  देऊन जाईल.......!

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
 
 
AHMED MUHAMMAD ELIAS
MECHANICAL ENGINEER
ASNT LEVEL II NDT INSPECTOR 
IRAQ :-+9647710951885,+9647503136603
PLEAS FEEL FREE TO CONTACT ME FOR ANY INQUIRY

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...