Re: [MW:8448] P no for SA-194 Grade 2H nuts

2H nuts shall not be welded to any pressure parts ( see UCS 4 or 5 of ASME Sec VIII Div 1 ) as it contains more than 0.35% Carbon.

arun

On Tue, Nov 30, 2010 at 2:42 PM, Shadab Alam Ansari <ansari@ghi.com.sa> wrote:

Dear All,

Which P. no shall be assigned to weld Nuts of SA-194 grade 2H?

Please provide your valuable comments.

 

Regards

Shadab

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...