Tuesday, November 30, 2010

Re: [MW:8438] Regarding high managanese steel Gr III WELDING

Sir, Pl note the trailing mail & advise for suitable consumable regards Nagbhushan. India

Sent from my BlackBerry® smartphone from !DEA


From: vinit vani <vinit_vani@yahoo.co.in>
Sender: materials-welding@googlegroups.com
Date: Tue, 30 Nov 2010 14:28:06 +0530 (IST)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:8437] Regarding high managanese steel Gr III WELDING

Dear all
 
I have two different issues.
 
1)we want to do hardfacing on  high manganese steel Gr III Base Metal.
    Please share your experience on MAG  Welding process for this material.
    Also please intimate any additional & valuable information regarding this.
 
2)Other issue is to know the  applicable ASTM  Std for High Strength Low Alloy Cast     Steel               for the chemical composition given below as well as supplier for this material in INDIA if any.
 

Mn - 1.4 to 1.8 %

Nb - 0.02 to 0.05 %

V - 0 - 0.06 %

Mo - 0.2 to 0.35 %

 c-0.10 to0.15%

 
Please reply me promptly because the matter is urgent.
 
Thanks & Regards
Vinit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...