Hi,
AWS doesnt require any PWHT.But if PWHT specified in Project specification,it shall be done as per AWS-Section 5.8
5.8 Stress-Relief Heat Treatment
Where required by the contract documents, welded assemblies
shall be stress relieved by heat treating. Final
machining after stress relieving shall be considered when
needed to maintain dimensional tolerances.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 11/24/10, mijin mathew mathew <mijinargentina@gmail.com> wrote:

From: mijin mathew mathew <mijinargentina@gmail.com>
Subject: [MW:8365] pwht thickness as per AWS D1.1
To: materials-welding@googlegroups.com
Date: Wednesday, November 24, 2010, 11:59 PM

Hi,
As per ASME B31.3 above 20mm thickness materials we are doing pwht.As per AWS D1.1, above which thickness we need to carryout pwht.???

Thanks & Regards
Mijin
Mumbai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...