In pipe line activities the joints which are not hydro tested are generally referred as golden joints.

These joints will come especially making tie-in’s of for 2 hydro test of sections.

I was experienced with the section as follows….

 

100 % NDT Is must in this case.

 

Option 1

1.      Root 100% DPT

2.      Every layer of weld with 100%DPT.

3.      Final run 100% DPT.

4.      100 % UT.

 

Option 2

1.      Root 100% DPT

2.      100 % RT

 

This is my personal experience

 

Thanks & Regards

 

Lakshman kumar.B | Manager - QA/QC | LANCO  INFRATECH LIMITED
Plot# 1255 | Sanjeevani Chowk | Mahanadi Vihar | Cuttack 753004

Phone : + 91-671-2445033| Mobile: +91 9937286851 | www.lancogroup.com

Go Green |The future will thank you

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of T. Mahendran
Sent: Saturday, October 30, 2010 1:42 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7936] golden weld joint require ments

 

Mr Gulam

 

I could remember the following things for Golden weld.

 

a) It means , other than of fabrication shop welding, the balance welding which will  be done with only one joint at site welding( or) in a tie -in work process. This type of joints are confirmed by 100% RT or UT (NDT), since there may be  a practice problem in the hydro test depends with the pipe  length.

 

b)There is no specific code for Golden joint but most of the companies are follow  to perform a "golden weld", with 100% NDT by eliminating hydro test.

 

c) We can refer  ASME 31.4, and  it  permits a "waiver" of a hydro test on “tie-in” welds between two sections of piping , that the weld has already undergone 100% NDT (see Section 437.1.4 (b) Testing Tie ins, ASME B31.4 2002 Edition).

 

T.Mahendran
KSA

 


From: Gulam kader <armvasi@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sat, October 30, 2010 9:42:49 AM
Subject: [MW:7933] golden weld joint require ments

Dear all,

can any one explain the golden joint welding , NDT and inspection requirement with Code references.

Regards,

Gulam Kader

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

Kumar said...

If 100% volumetric examination is done on golden joint by RT, then what is the purpose of root DPT?

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...