Re: [MW:7934] golden weld joint require ments




Golden Joint mean Tie in Joint.normally it will come on Piping final
joint . in this joint after welding you can not test hydrostatic test.
So you have to go for double NDT for volumetric such as RT / UT and MPT
/ DPT . After successful carrying out these test you can release the
joint for charging lines.


On Sat, 30 Oct 2010 12:45:30 +0530 wrote
>Dear all,

can any one explain the golden joint welding , NDT and inspection
requirement with Code references.

Regards,

Gulam Kader




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...