Re: [MW:7907] About electrode

Hi
 
Very interesting question.
 
May be feedability problem in the SAW & offset the main advantage of GTAW process if you use coated consumables.
 
Others can share their thoughts.
 
Regards,
 
K.Babu
Singapore
 
----- Original Message -----
Sent: Thursday, October 28, 2010 2:21 PM
Subject: [MW:7900] About electrode

Dear all,


i hv simple que.

we used coated electrode for SMAW so why don't we use coated filler wire for SAW & GTAW


Regards,
VIshal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...