Thursday, October 28, 2010

RE: [MW:7905] 9000 lbs thredolet

Check the attachment for #9000 Socket welded outlets, Threaded component are generally available/used up to #6000 only as stated by Mr Joseph

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bisso, Giuseppe
Sent: Thursday, October 28, 2010 11:57 AM
To: materials-welding@googlegroups.com
Subject: R: [MW:7902] 9000 lbs thredolet

 

As far as I know  threadolets s 9000 are not  generally allowed  (only socklolet or weldolet) : here the risk  of threading for high pressuie levels .

 

Joseph B.

 


Da: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Per conto di Ramprasad Chari
Inviato: giovedì 28 ottobre 2010 8.21
A: materials-welding@googlegroups.com
Oggetto: Re: [MW:7901] 9000 lbs thredolet

 

Mr Saurabh,

Thanks but Bonneyforge provides dimensions upto 6000LBS and not 9000 Lbs

Regards

aarpee

On Thu, Oct 28, 2010 at 11:28 AM, <ppefit@gmail.com> wrote:

Dear Mr. Aarpee,
You can find all the dimensions on bonny forge website.
Saurabh
Sent on my BlackBerry® from Vodafone


-----Original Message-----
From: Aarpee <ramprasad.chari@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Wed, 27 Oct 2010 22:40:03
To: Materials & Welding<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:7898] 9000 lbs thredolet

Can someone provide dimensions for 1/2" & 3/4" size 9000 Lbs
thredolet?
Thanks and Regards
Aarpee