Re: [MW:7235] Consumables to Base Metal

Hi,
ASME Sec.IX classified the electrodes as

QW-432.1 Steel and Steel Alloys

QW-432.2 Aluminum and Aluminum-Base Alloys

QW-432.3 Copper and Copper-Base Alloys

QW-432.4 Nickel and Nickel-Base Alloys

QW-432.5 Titanium and Titanium Alloys

QW-432.6 Zirconium and Zirconium Alloys

QW-432.7 Hard-Facing Weld Metal Overlay
with F.number.But there is no recommendation to use for the particular grade of material.Its your responsibility to select the proper consumables with the specifications given in ASME Section-II,Part-C to match with the properties of base metals and welding process.
 
Also you can refer with the Manufacturer's recommendations.
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 9/28/10, Larry <quality@unieng.com.au> wrote:

From: Larry <quality@unieng.com.au>
Subject: [MW:7230] Consumables to Base Metal
To: materials-welding@googlegroups.com
Date: Tuesday, September 28, 2010, 6:56 AM

Hi there,

 

Can anybody pointed me out to which clause in ASME IX that says that a certain consumables (Electrode) would be able to weld a certain base metal.

 

Your response is very much appreciated.

 

 

Thanks,

 

Larry

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...