Re: [MW:6303] API 1104 CODE ISSUE

Dear Limesh,
 
What is specification of 4130.  As per ASTM A 519 there are 4 grades of 4130.  Their yield strengths are for Hot rolled condition is 70 KSI, Stress releived condition is 85 ksi, Annealed condition 55 and Normalised condition 60KSI.  As per YS group of 1104 if YS less than equal to 65 KSI are under group 3.  So the welding between X 65 to 4130 can be used for X 60 to 4130 but not vice versa.    You can use E 8018 G /   ER 80SG / can be used for welding. 
 
Regards
 
N.V. PRASAD

On Wed, Aug 4, 2010 at 8:50 AM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Qualifying for higher grade will be the best choice.

--- On Tue, 3/8/10, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:6291] API 1104 CODE ISSUE
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Tuesday, 3 August, 2010, 6:36 PM


Dear All,

I need to qualify a welding procedure to API 1104, welding X60 pipe to
Gr. 4130 material. I would like to know if I can do this using a pipe
coupon that is "dual certified X60/X65", or would that pipe only be
usable to qualify an X65 procedure?What consumable I have to use in
this case?

Thanks and Regards


Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:27053] Required electrode for A335 P11 # S316 material

Is it advisable to weld Austenetic SS filler over Nickel base weldments? THANKS & BEST REGARDS, KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1, ...