Monday, August 30, 2010

[MW:6784] RE: 6769] Any WPS for P91 Material without PWHT

Not possible to qualify the P91 procedure with PWHT.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohamed Farook
Sent: Monday, August 30, 2010 9:30 AM
To: materials-welding@googlegroups.com
Subject: [MW:6769] Any WPS for P91 Material without PWHT

 

Dear friends,

 

Greetings to all,

 

Please advise me if you have WPS for P91 material without PWHT….

 

PWHT is time consuming..

 

Thanks and Regards,

asfaruk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...