Friday, July 30, 2010

Re: [MW:6210] API 653 Tank Repair

Dear all,
thanks for your reply.

these are defects identified by inspection team.

1. Fixed Roof - Remove the weld defects from the roof to shell angle and repair

2. Fixed Roof - Remove the weld defect from the butt weld adjoining Plates

3. Bottom - Puddle weld or install a lap-welded patch plate over the 0.150 inch deep internal pit on the sump bottom plate.

4. Bottom - Remove the corroded manual gauge repad/striker plate,


Regards,
Vijay.

On Fri, Jul 30, 2010 at 2:28 AM, ahmmad ali mohammed <ali47.alisha@gmail.com> wrote:
Dear Vijay
 
you are not given clear details about the location and type of repaire.
generally the following steps to be follow---
first thing is to ensure the type and depthe of defect by ndt methods as per site conditions.
if a repaire is crack
drill at the both ends of crack to prevent further propgation of crack  during grinding.
remove the defect by grinding only(gas cutting is not allowed).
after grinding ensure compleat removal of crack/slag etc by applying ndt methods
weld the cavity and apply final ndt (ut or rt) 
apply highly penetrating oil to ensure there is no leakage.
if necessary check the hardness value
 
i think this information may help you.
 
with regards
ahmmad ali 
 


 
On Sun, Jul 25, 2010 at 8:37 PM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear All,

We are going to carry out Repair of Diesel Storage Tanks as per API
653 specification.

Since am new to API 653, kindly guide me what are the things to be
carried out for Repair.

What are key points and what measures to be taken before carrying our
the repair.

Thanks in Advance. Kindly feed your inputs.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...