RE: [MW:6204] Weld-o-let welding minimum fillet size requirement

Complete bevel provided by mfr. to be filed (crotch). You may search earlier messages in the group on this subject.

sent from my handheld
-----Original Message-----
From: mubarish muhammed
Sent: 30/07/2010 4:56:32 pm
Subject: [MW:6203] Weld-o-let welding minimum fillet size requirement

Header pipe thickness is 41mm weldolet thickness 23mm , but other side
of weld-o-let 6mm. Please give me minimum weld metal for header to
weld- o-let joints whether we can weld less than 23mm & if going like
how much minimum fillet length required.

Mohd Mubarish.P.M
Abu Dhabi.
Welding Engineer.
CSWIP-3.1

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...