RE: [MW:6172] SAW Wire Test certificate review

You must have the mechanical test report in order to verify the type of flux used. Alloying or non-alloying.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eng/ Mostafa Kamel Hussein
Sent: Wednesday, July 28, 2010 1:57 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6166] SAW Wire Test certificate review

 

 

It's must to review the chemical analysis and mechanical properties according to ASME II part C, although ESAB is reputed mark, but it's mandatory that the electrode certificate contains the chemical and mechanical

 

SaSa


From: krishna <wiqw@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Mon, July 26, 2010 9:07:07 PM
Subject: [MW:6133] SAW Wire Test certificate review

Frnds,
Here i received one SAW Wire test certificate for ESAB OK AUTOROD 12.22L ,as per ASME SEC II Part c SFA 5.17 EM12K.

In the Test certificate they gave only Chemical Analysis of the wire .

Shall I accept the Test certificate or I have to ask for Mechanical Properties also.

Is it acceptable the Test certficate as it is.

Kindly guide,

thanks,
KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...