Tuesday, July 27, 2010

Re: [MW:6139] HSLA Welding.

these steel are refinement by adding microalloys such V,Al,Nb,Ti & thermo mechanically heat treatment to increse toughness & strength simultanously.
HY-80,HY-100 & X-100 are examples of these steels.
during of welding of these steels, the minimum H.I SHALL BE USED to prevent growth grain.


From: limesh M <limesh78@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Tue, July 27, 2010 10:15:16 AM
Subject: [MW:6137] HSLA Welding.

Dear All,

I have heard a lot about of HSLA(High Strength Low Alloy) and it
confusing me a lot.

Can anyone give a proper defenition for HSLA steel ?

What are all the common grades in API,ASME,ASTM,AISI comes under HSLA
steel category ?

HSLA-65 and API X65 are same material?

What are all the precautions we have to follow during HSLA welding ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...