Hi!

 

As base metal is of LAS ,  req  PWHT at min 650C  , Therefore suitable  consumable for clad restoration of 410 S clad is  E NiCr fe3 or NiCr Mo3

 

Preheat Temp . of base metal for barrier layer is 100 C , (No need of preheating  for subsequent layers.  min ,Interpass temp  is  175 max,  Welding Current – 110-120  Amp for 3 .2 dia electrode.

 

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of P.Rao
Sent: Saturday, June 26, 2010 5:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:5751] Welding of SA 240 TP 410S material.

 

Dear all,

Can any body share the experience in welding of SA240 TP410 Material.

I have a Vessel consists SA387 Gr.11 Cl.2 material cladded with SS410S.

Internal Piping material : SS410S thickness 10-15mm.

Construction Code : ASME SEC VIII Div.1.

Welds in SS410S will under PWHT of low Low alloy steel.

Need guidance in Preheat & interpass temperature of SS410 material welding (Consumable selected for welding of SS410S is 309L type).

regards

P.Rao

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...