Sunday, May 30, 2010

Re: [MW:5292] Tack welder test

Rutvik,
Check AWS D1.1 clause 4.31 Method of Testing and Acceptance Criteria for Tack Welder Qualification. clause 4.19.2,figure 4.39 and 4.35.

Best regards

BABU.P.R
mobile: +971509684056


--- On Thu, 27/5/10, rutvik dixit <rutvikdixit@yahoo.co.in> wrote:

From: rutvik dixit <rutvikdixit@yahoo.co.in>
Subject: Re: [MW:5276] Tack welder test
To: materials-welding@googlegroups.com
Date: Thursday, 27 May, 2010, 11:00 PM

Hi Gulam Kader,
You can go for fillet weld test. You may refer ASME sec.IX, article III  if it is applicable to your project.


With Regards,
Rutvik
Sr.Surveyor
TATA Projects Ltd.

--- On Thu, 27/5/10, Gulam kader <armvasi@gmail.com> wrote:

From: Gulam kader <armvasi@gmail.com>
Subject: [MW:5270] Tack welder test
To: materials-welding@googlegroups.com
Date: Thursday, 27 May, 2010, 6:03 PM

Hi to all,

Please explain how to qualify the welder only for tack weld  with code reference.

Regards,

GKM
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...