Dear All,

I just want to join two pipes of ASTM A106 Grade B. As per project
speification CE(Carbon Equivalent) permitted as per IIW formula is
0.43 I found that there is no silicon participation in this
formula.But I have come to know that API RP 577 Clause 10.9.1 using a
formula which includes silicon and rest of the part is equivalent to
IIW formula.If we review the standard for ASTM A 106 Grade B for
chemical properties(Table 1 Chemical requirements);we can observe that
the chemical composition has no restriction for silicon (min 0.10 for
all grades) .ie, there is no maximum limit !!! Can we accept
technically an ASTM A 106 Grade B mill certificate with silicon
content ranging from 0.10 to UNLIMITED ??? If not what would be the
maximum acceptable silicon percentage in A106 Grades ?

Thanks and Regards

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...