Dear Manoj,

LR Grade A material is a structural rolled steel grade according to
Chapter 3 section 2 of the Lloyd's Register Rules for Manufacture,
Testing and Certification of Materials.
This material has the following chemical composition: C max. 0.21% ;
Mn min. 2.5 x %C ; Si max. 0.50% ; P max. 0.04% ; S max. 0.04%
Mechanical properties are: Yield Strength min. 235 MPa ; Tensile
Strength 400 - 490 MPa ; Elongation min. 22% and has no Chapy-V impact
requirements.

Best Regards,

Herman Pieper

On 23 mei, 18:00, manoj john <manojac...@gmail.com> wrote:
> Dear All
>
> Can anybody give info about LR  A grade material
>
> Thanks & Regards.
> Manoj
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...