Thursday, April 22, 2010

RE: [MW:4923] Purging

BOC
Do have NEW purging device that makes it far easier plus saves a fortune on
gas
Best Regards

PHIL CHEW
Global Segment Manager -Transport ,Shipbuilding,M&R

ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB

Tel: +44 (0) 7584 219132

email: PHIL.CHEW@esab.net

ESAB Holdings Ltd is a company registered in England and Wales . Co
registration no 1687590
Registered Office: 322 High Holborn, London , UK , WC1V 7PB
www.esab.com
Please consider the environment before printing this email.



"Bathula Raghuram
(Mumbai -
PIPING)" To
<R.Bathula@ticb.c "materials-welding@googlegroups.com
om> "
Sent by: <materials-welding@googlegroups.com
materials-welding >
@googlegroups.com cc

Subject
22/04/2010 10:41 RE: [MW:4921] Purging


Please respond to
materials-welding
@googlegroups.com


Yes, you can.

From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Ramesh Barot
Sent: Thursday, April 22, 2010 2:38 PM
To: Materials Welding
Subject: [MW:4918] Purging

Dear All,

I have one doubt for purging of ss material. If we have inside excess for
back chip then can we allow to do welding without purging in all cases?

Thanks,
With Best Regards,
Ramesh Barot


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

----------------------------------------------------------------------------------
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.

ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Subscription settings: http://groups.google.com/group/materials-welding/subscribe?hl=en

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...