Dear Syah,
For the A53 GrB this specification for pipe, steel, black and hot dipped, zinc coated, welded and seamless. It itended for mechanical and pressure application.
And for the A106 GrB this specification for seamless carbon steel pipe for high temperature service, it suitable for bending, flanging, and similar forming operation and for welding.

Brg

Hong Ky Thai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...