Saturday, March 13, 2010

Re: [MW:4558] colour of welding after SAW welding in low alloy mild steel

This is due to the Travel Speel and fast cooling , the flux is remove immediately as it is formed .
 
Maintain the PRe heat and interpass Temp and dont remove the flux till it get ditached fromt he surface .
 
Thanks
 
Sujeet

On Sat, Mar 6, 2010 at 6:33 AM, raw <rohit30584@gmail.com> wrote:
Hi there,
I have a query related to the colour of welding .After doing SAW
welding on pre conrac machine in low alloy mild steel , the colour of
welding sometimes comes out to be blue or yellowish-blue.Is this a
kind of defect or due to some another reason.Please clarify.
Rohit Rawat(QA),
Kirby Building Systems,
Haridwar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...