No as long as sufficient details are given in the TC for establishing that
it conforms to the specification.

Regards,

Abu Rehan Abbasi
+965-97274238
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of qaqcmpm
Sent: Wednesday, March 31, 2010 6:50 AM
To: Materials & Welding
Subject: [MW:4637] SA965/SA788

while reviewing the MTC for SA965, it states

3.2 Material supplied to this specification shall conform to the
requirements of Specification A 788

If the MTC does not have mentioned SA788, is it a non conformance?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...