Re: [MW:4152] ASME SEC IX...PWHT?

ASME IX is not a code that can determine the PWHT, you must use a code of construction like being ASME B31.3 or ASME VIII. Soon you must determine N° P and the group that ASTM A333 corresponds, since there are different considerations for what has been said
Ruscitto

>>> Nandesh Kumar <nandeshkumar@rocketmail.com> 26/01/2010 06:33 am >>>
Dear All,
 
For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.
Material is ASTM A333 .
 
Thaks in advance
Nandesh Kumar A


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

*********************************************************************

¡IMPORTANTE!

Para evitar accidentes por inhalación de monóxido de carbono:

- Mantenga los ambientes ventilados en forma permanente.

- Revise que la llama sea color azul y uniforme.

- Instale y haga revisar periódicamente sus artefactos sólo a través de gasistas matriculados.

Recuerde que los artefactos a gas pueden emitir Monóxido de Carbono: un gas altamente tóxico e imperceptible.

Más consejos en http://www.metrogas.com.ar

*********************************************************************

Este mensaje es privado y confidencial y va dirigido sólo al destinatario indicado. Si lo ha recibido por error, por favor avísenos inmediatamente vía e-mail a error-mail@metrogas.com.ar y tenga la amabilidad de eliminarlo de su sistema. La utilización o divulgación de su contenido puede importar la comisión de un delito. No copie, reproduzca o divulgue -en forma parcial o total- su contenido. Cualquier opinión contenida, es exclusiva de su autor y no representa la opinión de MetroGAS S.A. - Muchas gracias.

This message is private and confidential and it is only intended for the addressee named above. If you have received this message and it is not addressed to you, please advise us immediately at error-mail@metrogas.com.ar and kindly remove it from your system. The use or disclosure of its contents may be regarded as an offense. Do not copy, reproduce or disclose them, either partially or fully. Opinions are the exclusive responsibility of the author and do not represent the opinion of MetroGAS S.A. - Thank you.

:: http://www.metrogas.com.ar

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...