Re: [MW:4114] Low hydrogen electrodes for station piping

because low hydrogen is a stronger weld material and less hydrogen content so less cracking in the weld and heat afected zone area.
 
 
regards
mike.
----- Original Message -----
Sent: Wednesday, January 20, 2010 9:54 AM
Subject: [MW:4104] Low hydrogen electrodes for station piping

Dear all,
 
why we are always using low hydrogen electrodes for station piping instead of cellulose electrode. somebody can explain please?
 
Regards,
 
Gulam Kader


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.432 / Virus Database: 270.14.151/2633 - Release Date: 01/19/10 17:49:00


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...