dear sir anything biger than the calaberation notch wich is 1mm is a defect and i do believe it would be down to the welding engineer to make a desision as to wether or not to use the elbow i do bilieve that there is no specific area as to how much pitting would b allowed the decision would be yes or no or can the pitting b eliminated i.e repair welded as a welding inspector i would have some idea as to wether or not it way be used but would hafto come from a engineer and depending on what product would be going through the material
 
 
regards
mike.
----- Original Message -----
Sent: Wednesday, January 20, 2010 9:52 AM
Subject: [MW:4105] Pitting acceptance criteria

Dear all,
 
We received one 40" elbow (ASME 16.9) ASTM A 860 material having so much pitting on full external surface. Which standard we can refer for the acceptance criteria? 
 
 
I referred in ASTM A 860, its talks about only depth of surface discontinuity(5% of the nominal thickness),  there is no detail about the area of the pitting allowance.
 
Please help me on this issue. Very urgent
 
Regards,
 
Gulam Kader 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.432 / Virus Database: 270.14.151/2633 - Release Date: 01/19/10 17:49:00


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...