Hi,
     PMI values are not exact value, so the below value of Mn is not a major problem. If you want confirm the correct value, select the wet analaysis method.
 
Louis
Welding Inspector
Singapore

--- On Tue, 19/1/10, babu k <kbabupsg@gmail.com> wrote:

From: babu k <kbabupsg@gmail.com>
Subject: Re: [MW:4092] composition manganese less than requirment of ASTM A36
To: materials-welding@googlegroups.com
Date: Tuesday, 19 January, 2010, 7:44 PM

Hi,
 
The reduction in Mn may be compensated by Carbon content,
 
Also the exact Mn content value u can cross check with wet analysis.
 
 
 


On Mon, Jan 18, 2010 at 11:52 AM, Tran Van Vuong <vuong.tv@gmail.com> wrote:

Dear All,

 

Please help me in PMI testing for material ASTM A36 thickness over 20.0mm, the composition requirement of manganese is (0.8 – 1.2)%. But result of test is less than 0.8%. Other testings are accepted (tensile, bending, elongation).

 

Please advice me this result is accepted or not.

 

If not, please advice the solution.

 

Thank you in advance.

 

TRAN VAN VUONG
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...