hi

to select the process we have to know the shedule. ;prefered process is GTAW. IF THE SHEDULE IS HIGH THAN GO FOR GTAWW + SMAW. ELECTRODE IS 316L FILLER AND ELECTRODE.

THX & RGDS
M.M.REDDY
mog_mahendra@rediff.com
0020198687114

note : willson friend reddy.

On Sat, Dec 26, 2009 at 9:26 AM, Ohm-Srinivasulu. K <nirgunaya@yahoo.com> wrote:
Hi,
 
I want to weld SS316 DIN W.N flange SS304 Pipe,
could anyone tell me what kind of welding is prefered and electrodes.
 
Thanks
Srinivas
 
 
 
 
 
 


ohm guru namasivaya

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...