Dear Ganesh,
Constant current power sources are preferred in the process where the control is manual. e.g SMAW so that if at all there is variation in the arc length in welding it implies variation in the voltage but the current remain almost constant. But whereever machine operation  is possible generally constant Voltage power sources are preferred
 
Amarjit Singh
TEMA INDIA LTD

On Sun, Dec 13, 2009 at 6:40 PM, ganesh kumar <mgkumar29@gmail.com> wrote:
Hello friends
      I had an doubt regarding the power source. Why DC-CC power source is not preferred in SAW process.
Due the voltage variations or any other specific reasons
kindly reply me if any one knows  the answer

--
Ganeshkumar M

Mobile: 9442510888

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Amarjit Singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...