[MW:3879] Welding of Cast iron overlay by GMAW/FCAW

Dear All
Good Day
 
Which will be the Best suitable fillerwire for Overlay of Castiron by GMAW/FCAW ?
At present it is been done by stick using E-NIFeCI SFA 5.15.
 