RE: [MW:3751] Welding of SA 537

SMAW

Air Liquide/Oerlikon Tenactito 38R for SMAW (E7018-G)
Air Liquide/Oerlikon SD3 Wire/ OP121TT Flux for SAW

Excellent low temperature impact test properties with 450MPa yield approx.

Regards
Robert

-----Original Message-----
From: KC [mailto:kc.chavda07@gmail.com]
Sent: 26 November 2009 12:03
To: Materials & Welding
Subject: [MW:3750] Welding of SA 537

Can anyone tell me to weld the below material with SMAW which
electrodes we have to use , to weld with SAW which filler wire & flux
combination we have to use.
The material and test requirement is as below…

 Material is SA-537 Class 1, Fully Killed, Normalized, Charpy V-
Impact Tested
 Material is SA-516 Gr.70, Fully Killed, Normalized
 Thickness varies from 38 mm to 50 mm for both materials.
After complication of welding we have to test PTC (production test
coupon) @ -48˚C (Negative 48). The impact energy value shell be 50
joule.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This email message and accompanying data are for the sole use of the intended recipient(s) and may contain confidential information and/or copyright material. Unauthorised use, copying or disclosure of any of it is prohibited and may be unlawful. If you received this email message in error, please notify us immediately and erase all copies of this message and attachments. Global Energy scans and monitors incoming and outgoing mail in accordance with its IT Policy - this email has been scanned for viruses. Global Energy Holdings Ltd and its subsidiaries accept no liability for direct, indirect or consequential damages arising from the alteration of the contents of this message by a third party, or as a result of a virus being passed on.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...