Re: [MW:3710] RE: 3694] damage of packing material of SW valve after PWHT at site

HiVinayak,

Rahul is right, but i think you already purchased all the valves without puff pieces. so you can minimize the heat input at gland packing areas by wound the heating coil around the joint only and avoid over valve body and keep open the gland packing (bonet area) for air circualtion/contact which will desipate the heat. During pwht time keep open the gate to avoid damage to valve seat.

Also you can carriout some trial hydrotest for valves with gate 1/2 open condition to verify the gland packing condition. In my perious project i had done some random test and there was no leakage observed that time.




On Fri, Nov 20, 2009 at 12:08 PM, Pisat, R. R(ahul) <Rahul.Pisat@akzonobel.com> wrote:
hi Vinayak,
 
You are very much right regarding damage to the valve packing .
These SW valve shall be procured with 100 or 150 mm Puff ( a piece of pipe ) welded on both side by.
 
PWHT at valve end shall be done by manufacturer.
 
hope it clarifies.
 

Kind regards

Rahul



From: Nivendkar Vinayak (Mumbai - Piping) [mailto:V.Nivendkar@ticb.com]
Sent: vrijdag 20 november 2009 7:34
To: piping_valves@yahoogroups.com; materials-welding@googlegroups.com
Subject: [MW:3694] damage of packing material of SW valve after PWHT at site

Dear all,
 
In the piping class of alloy steel, we have SW end small bore gate, globe valves. And as per the client requirements all Alloy steel piping joints shall be PWHT after welding.
 
Now , if we performed the PWHT at site at temp. 704-760 Deg C (As per ASME B 31.3 Table 331.1.1 Requirements for heat treatments), then is there any possibility of damage to packing material which is normally graphite due to heat dissipate during PWHT.
 
What type special consideration to be taken in this case. Members are requested to give suggustions.
 
Thanks in advance..
 
Regards,
Vinayak


____________________________________________________________________________
This email has been scanned for Viruses and Spam. For more information
please contact your local Business Unit Information Security representative.
____________________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Regards,

Mohan, Q8.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...