Re: [MW:3697] damage of packing material of SW valve after PWHT at site

If the valves are 'bolted bonnet', consider the disassembly of the valves before PWHT.  If the bonnet is welded to the body of the valve, investigate if a preheat will fulfill your design requirements. 

Alternatively, restrict the rate of heat input during welding by limiting the size of electrode  (SMAW) and the amperage setting. Also limit the interpass temperature and weld bead width.    

Regards,
Darcy Morin



On 2009-11-19, at 23:34, "Nivendkar Vinayak (Mumbai - Piping)" <V.Nivendkar@ticb.com> wrote:

Dear all,
 
In the piping class of alloy steel, we have SW end small bore gate, globe valves. And as per the client requirements all Alloy steel piping joints shall be PWHT after welding.
 
Now , if we performed the PWHT at site at temp. 704-760 Deg C (As per ASME B 31.3 Table 331.1.1 Requirements for heat treatments), then is there any possibility of damage to packing material which is normally graphite due to heat dissipate during PWHT.
 
What type special consideration to be taken in this case. Members are requested to give suggustions.
 
Thanks in advance..
 
Regards,
Vinayak

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...