Wednesday, November 25, 2009

Re: FW: [MW:3734] NDT procedure qualification

I agree with Mr.Pradip who has given a very elaborate details.
While demonstrating one thing to be remembered is to perform the demo
on a mock up with known flaws, ie., the fingerprints of the flaws of the
specimen should be available with NDT Level III so that validation of
the technique can be established.

Thanks and regards,
Raghavendra Pemmaraju
ASNT NDT Level III (RT,UT,MT),PCN L-II (UT,Phased Array UT),RSO L-III
(BARC)
Senior Manager,QC
Heavy Engg.Division,
Larsen & Toubro Limited
Hazira Manufacturing Complex
Surat, Gujarat
India

Larsen & Toubro Limited
www.larsentoubro.com

This Email may contain confidential or privileged information for the
intended recipient (s) If you are not the intended recipient, please do
not use or disseminate the information, notify the sender and delete it
from your system.


>>> <pgoswami@sympatico.ca> 25/11/2009 03:59 am >>>



Subject: RE: [MW:3725] NDT procedure qualification
Date: Tue, 24 Nov 2009 14:52:24 -0500
From: pradip.goswami@opg.com
To: pgoswami@sympatico.ca

Dear Hrishi,

Demonstration of NDT procedure is a requirement to ensure that correct
technique is adopted which concurs with the written NDE procedure. Any
NDE procedure has a host of variable, operators training, equipment
calibration, if required NDE mock ups etc. Any of the missing variables
may affect the quality and results of NDE inspection. Hence it is always
advisable to check the correctness of proper NDE technique, prior to
actual NDE on the job.

If you read through ASME Sec-V each NDE technique requires to
satisfactorily establishing prior to application in the job. Usually
this has be ensured by an ASNT Level--II or Level- III personnel or
persons with equivalent NDE qualification.

In ASME Sec-V the following articles talks about demonstration
/qualification: --

* T-221.2 Procedure Demonstration.*Radiography.
* T-721.2 Procedure Qualification*MPI
* T-421.2 Procedure Qualification.-- UT
* T-621.2 Procedure Qualification.--LPI


Hope it answers your query.

Pradip Goswami,P.Eng
Senior Engineer/Specialist(Welding-Metallurgy)
Machine Dynamics & Component Integrity Dept.
Engineering & Training Services Division
ONTARIO POWER GENERATION Inc.
PO Box-2000, RR-55(South)
Nanticoke, Ontario,N0A1L0
Tel:-(519) 587-2201, Ext 3107--in Nanticoke
(416) 231-4111, Ext 5925--in Kipling,Toronto
Fax: (519) 587-6814
Email-pradip.goswami@opg.com.

Date: Tue, 24 Nov 2009 18:21:16 +0530
Subject: [MW:3725] NDT procedure qualification
From: hrishikm07@gmail.com
To: materials-welding@googlegroups.com

Is it mandatory to demonstrate NDT procedure qualification before
applying in the actual job? If so, please give the code/standard
reference.

Regards

Hrishi

--
To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S)
AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR
CONFIDENTIAL. If you are not the intended recipient, you are hereby
notified that any review, retransmission, dissemination, distribution,
copying, conversion to hard copy or other use of this communication is
strictly prohibited. If you are not the intended recipient and have
received this message in error, please notify me by return e-mail and
delete this message from your system. Ontario Power Generation Inc.

--
To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe
from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...