Wednesday, October 28, 2009

[MW:3556] acceptance crerteria of undercut

Hi dear

Please let me know that according to iso 5817 rev: 2005 class C the undercut with 0.2mm depth and 24 mm length in Butt Weld and 100 mm length of our product is acceptable or not.if yes or no please explain exactly with detail.

 

Best regards

Alireza Samimi



__________ Information from ESET NOD32 Antivirus, version of virus signature database 4530 (20091021) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...