[MW:3501] Re: Welding of Sa-335 to SA-106

Dear  jimmy,
 
Pl. refer   UW 424  in ASME section   IX, IF you have a PQR for  Base  material P4 to P4, You can  use  for  P4 to  P4 or  P3 or  P1.
 
Also, you have  to  see  other  essential variable.
 
Regards,
Paresh
 

Date: Mon, 12 Oct 2009 20:18:46 +0400
Subject: [MW:3495] Re: Welding of Sa-335 to SA-106
From: ibratech@gmail.com
To: materials-welding@googlegroups.com

Hi,
 
You cannot use that PQR. Change in P number is essential variable.
 
Regards,
Ibrahim

2009/10/12 Jimmy Nielsen <nielsen.jimmy@gmail.com>

Hello Gents

Can sombody help me with a answar regarding welding of Sa-335 to
SA-106.

I have a PQR covering material 335-P11 to 335-P11( P4)
Can I use it for welding of P-no 4 to P-no 1

Regard, jimmy





--
Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...