Monday, October 12, 2009

[MW:3487] RE: 3479] S-Number

S numbers were materials approved by B31 committees but did not have allowables in Sc. II and were not approved for use in Sc I or Sc VIII construction.  Often used for construction of hangers and hanger assemblies for piping that was governed by B31 but not in pressure boundary use.
 
John


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Sunday, October 11, 2009 1:00 AM
To: materials-welding@googlegroups.com
Subject: [MW:3479] S-Number

Hi Friends

As per ASME Sec.IX, QW420, materials are grouped and assigned P-Numbers i.e. Parent material number.

Similarly i would like to know what is meant by S-Number with full form and detailed explanation !!!


Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...

Pages

Contributors

Blog Archive